Analysis of Fully Refined Paraffin Wax 0.5% Oil Content |
Test |
Test Method |
Result |
Oil Content |
ASTM D 721 |
Max 0.23% |
Flash Point |
ASTM D 92 |
Minimum 250 c |
Melting Point |
ASTM D 87 |
67 c |
Congealing Point |
ASTM D 938 |
66.8 c |
Color |
IP 17
Method A 2 Cell
|
0.1 Y |
Kinematic Viscosity @ 100 c |
ASTM D 445 |
6.2 cst |
Refractive Index @ 90 c |
|
1.43177 |
Needle Penetration |
ASTM D 1321 |
14 (0.1 mm ) |
Semi-refined Paraffin Wax (1-2%)
CHARACTERISTIC |
RESULT |
METHOD |
Oil content |
1-2 % wt |
ASTM D-721 |
Melting Point |
64-68 ◦C |
ASTM D-87 |
Flash Point |
220-240◦C |
ASTM D-92 |
Kinematic Viscosity at 100◦C |
6-7.5 CST |
ASTM D-445 |
Color (Lovibond) |
White |
Method (2″ cell) |
Semi-refined Paraffin Wax (2-4%)
CHARACTERISTIC |
RESULT |
METHOD |
Oil content |
2-4 % wt |
ASTM D-721 |
Melting Point |
62-66 ◦C |
ASTM D-87 |
Flash Point |
220-240◦C |
ASTM D-92 |
Kinematic Viscosity at 100◦C |
6-7.5 CST |
ASTM D-445 |
Color (Lovibond) |
White |
Method (2″ cell) |
Semi-refined Paraffin Wax (5-7%)
CHARACTERISTIC |
RESULT |
METHOD |
Oil content |
4-6 % wt |
ASTM D-721 |
Melting Point |
62-65 ◦C |
ASTM D-87 |
Flash Point |
220-240◦C |
ASTM D-92 |
Kinematic Viscosity at 100◦C |
6-7.5 CST |
ASTM D-445 |
Color (Lovibond) |
Yellowish White |
Method (2″ cell) |